http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20000041672-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_160494dd050ef58528168a9b2f7373c9 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C21C5-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B9-20 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B9-20 |
filingDate | 1998-12-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_eb7f5f27790bcd1b0b5042ba827dd29e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_14737aa682906d833eb17f9f3a395674 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_439d84c494488044eab14ff8c983888a |
publicationDate | 2000-07-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20000041672-A |
titleOfInvention | High speed melting method in electric furnace |
abstract | The present invention relates to the operation of the electric furnace, the melting method first determines the amount of the charge to be charged, the apparent specific gravity defined by (weight of the charge) / (over-factor × volume of the electric furnace) is 0.6 ton / ㎥ or less After charging 10-20% of the total amount of solid iron source, charge a certain size mold line in the range of 50-100% with respect to the amount of solid scrap, and then sequentially charge the solid scrap and the mold line in the same manner. Then, it comprises a dissolving, this dissolution method of the present invention can dissolve the charge at high speed by reducing the charging time and heat loss in one charge. |