Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0efa077d881a96aeb1e29b21ef1bbb58 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D123-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D7-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D123-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D123-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D123-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L35-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-20 |
filingDate |
1997-05-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8782dbf9da7a962c29026b5f1de771b2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4fcd8383503ddf12021b4a0a9afc7117 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_951d1e56e14754a17a2b4b25be45147d |
publicationDate |
2000-03-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-20000015909-A |
titleOfInvention |
How to temporarily protect the surface with a polymer coating |
abstract |
The present invention provides a solid polymer coating on the surface to be protected after application of an aqueous dispersion of a polymer of a) at least one C 2 -C 10 olefin and b) at least one comonomer which can be copolymerized with olefins under free conditions. Wherein the coating is directed to a method of temporarily protecting the surface, characterized in that the average dry thickness is greater than 20 μm and to the use of colored polymer dispersions and designs for temporary protection of the surface or for coloring the surface. |