Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c4b5184b7a8fe02a0c2cc4e509230214 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2367-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2423-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L67-03 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-101 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 |
filingDate |
1998-08-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5c68310e553689227534dc11b0ad16d6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d9611767e1674602212dc8cac131a026 |
publicationDate |
2000-03-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-20000015434-A |
titleOfInvention |
Polymer film |
abstract |
The present invention relates to a polymer film, wherein the polyester resin having an intrinsic viscosity of 0.5 to 0.9 dl / g composed of ethylene terephthalate of 60 wt% or more has a melt index of 1 to 20 (g / 10 minutes) and a melting point of 140 to 180 The polymer film of the present invention to which 5 to 20% by weight of polypropylene resin, 1 to 5% by weight of acrylate compound and 3 to 10% by weight of methyl acrylate compound is added, has a mechanical texture, It is excellent in light weight and post processing and can be widely used in various applications. |