http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-19990054955-A
Outgoing Links
Predicate | Object |
---|---|
filingDate | 1997-12-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 1999-07-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-19990054955-A |
titleOfInvention | Method for producing nylon 6 fibers by high speed spinning |
abstract | The present invention is a method for producing nylon 6 fibers, characterized in that the production of high-speed spinning at 5,000 m / min or more by adding 0.001 to 0.05% by weight of aluminum stearate or cobalt stearate to a dry nylon 6 polymer.n n n The present invention can produce yarns having a low frequency of trimming and curvature during spinning and excellent cross-sectional uniformity. |
priorityDate | 1997-12-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links