http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-19990042603-A
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2451-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2325-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L25-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L51-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2300-22 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K7-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K9-06 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-08 |
filingDate | 1997-11-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 1999-06-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-19990042603-A |
titleOfInvention | Styrene-based thermoplastic composites with improved impact strength |
abstract | The present invention is (A) 50 to 95 parts by weight of a styrene thermoplastic resin, (B) 5 to 50 parts by weight of inorganic reinforcing material and (C) 20 to 99 parts by weight of an aromatic vinyl monomer in 1 to 80 parts by weight of the rubber polymer graft 0.1 to 2 parts by weight of the organic peroxide and 0.1 to 10 parts by weight of the reactive monomer containing an epoxy group by melt kneading to 1 to 50 parts by weight of the modified vinyl aromatic graft copolymer to 100 parts by weight of the polymerized graft copolymer. It relates to a styrene-based thermoplastic composite material, characterized in that the impact strength improved. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100475009-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100884613-B1 |
priorityDate | 1997-11-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 82.