http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-19990021940-A
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2002-85 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-80 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09C1-0084 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09C1-0081 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09C1-0009 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09C1-00 |
filingDate | 1997-03-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 1999-03-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-19990021940-A |
titleOfInvention | Manufacturing method of inorganic pigment |
abstract | The present invention is composed of composite oxides of various elements, which are excellent in weather resistance and heat resistance, and are inorganic pigments having various color tones widely used in ceramic colorants, paints and synthetic resin colorants. A sufficiently developed composite oxide pigment can be obtained to achieve a simplification of the grinding process. In the manufacturing method of the inorganic pigment which mixes the oxide of the element which comprises a specific inorganic pigment, or the compound which becomes an oxide by applying heat in predetermined | prescribed ratio, and bakes the compounding raw material, A blending raw material is grind | pulverized instead of the said mixing process. Dry treatment is carried out to give sufficient energy to cause the mechanochemical reaction to the blended raw material, and the raw material particles are joined to coexist in the proportion of the blended raw material. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20020097083-A |
priorityDate | 1996-03-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 68.