abstract |
The present invention is a high-fluidity cementless filler comprising ferronickel slag (FNS, Ferro-nickel slag), water and a binder, wherein the binder includes bottom ash and an irritant, and the weight ratio of the binder and water is 1: 0.48 to 0.52, the weight ratio of the stimulant to the bottom ash is 1: 0.15 to 0.30, and the weight ratio of the binder to the ferronickel slag is 1: 0.5 to 0.6. will be. |