http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102375984-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B65H2701-1752 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B65H18-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B65H75-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B65H18-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B65H18-16 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65H18-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65H18-26 |
filingDate | 2016-09-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2022-03-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2022-03-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-102375984-B1 |
titleOfInvention | Polyvinyl alcohol film roll |
abstract | A roll formed by winding a PVA film having a thickness of 45 µm or less and a length of 2,000 m or more, wherein the average spacing between adjacent films is 5 µm or less; And, as a method of manufacturing a roll in which a PVA film having a thickness of 45 μm or less and a length of 2,000 m or more is wound, a touch winding method is employed, and the pressure between the film roll and the contact roll is 1 m in the axial direction of the film roll. Sugar is 3 to 30 N, and the winding speed is set to a manufacturing method of 30 m/min or less. Thereby, even if it is a case where a PVA film is thin and winding length is long, wrinkles and eccentricity do not generate|occur|produce easily, and the roll of a PVA film with a favorable external appearance is provided. |