http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102359260-B1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f984d8b1d7ecdc4d5253a7254e634ebf |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2103-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-91 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B20-004 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B20-0076 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B14-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B18-141 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B16-0641 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B20-008 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B22-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K17-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B20-0036 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B22-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B14-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B20-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K17-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B16-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B18-14 |
filingDate | 2021-04-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2022-02-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3e3db2c79398bb38c34c4bf8b81ae47a |
publicationDate | 2022-02-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-102359260-B1 |
titleOfInvention | Solidifying agent composition for soft ground and method for stabilizing soft ground using the same |
abstract | The soft ground stabilization method using the hardener composition for soft ground includes the steps of collecting raw alumina, bringing in the hardening agent composition, mixing and stirring the raw alumina and the hardening agent composition to prepare mixed soil, mixed soil Containing the steps of transporting and installing the mixed soil, compacting the installed mixed soil, and curing the minced mixed soil, the solidifying agent composition is a limestone by-product, blast furnace slag powder, cement, carbon material and particles and fibers containing a plurality of holes Including a reinforcing agent, the limestone by-product includes CaO, SO 3 , the particles including a plurality of holes are made of silica-alumina balloons, and the particles including a plurality of holes are the first particles, the second particles and the third comprising particles, the first particle having a diameter of 50 μm to 65 μm, the second particle having a diameter of 66 μm to 80 μm, and the third particle having a diameter of 81 μm to 90 μm, and the fiber reinforcing agent comprises PVA fibers However, the fiber reinforcing agent is heat-treated at 195° C. for 3 minutes and then dried at room temperature for 35 minutes, the solidifying agent composition further includes an accelerator made of calcium carbonate, and the blast furnace slag powder contains 2.9% to 3.5% MgO, , 1.3% to 1.8% SO 3 , 0.004% to 0.009% of chloride ions, wherein the blast furnace slag powder has a basicity of 1.65% to 1.72%, a density of 3.12 g/cm 2 to 3.18 g/cm 2 , and 4,015 cm 2 It has a specific surface area of /gr or more and a flow ratio of 99 to 108%, and the carbon ash includes non-magnetic coal fly ash. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102518138-B1 |
priorityDate | 2021-04-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 45.