http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102350899-B1

Outgoing Links

Predicate Object
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/E04F15-12
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-16
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/E04F21-04
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D175-04
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D133-04
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-16
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/E04F15-12
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/E04F21-04
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D175-04
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D133-04
filingDate 2019-12-23-04:00^^<http://www.w3.org/2001/XMLSchema#date>
grantDate 2022-01-14-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationDate 2022-01-14-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber KR-102350899-B1
titleOfInvention The painting method of reinforce, protect humidity and pattern on surface of the fioor
abstract The present invention relates to a method for reinforcing moisture-proof floors and painting patterns. A step of applying a top coat of 'Poly Top', which is a polyurethane-based paint having an optional background color, to the surface of the cured undercoat layer, and reinforcing the floor with moisture proof reinforcement by the cured top coater layer. Moisture proof reinforcement of the floor and: The process of applying a second coat of 'M, M, A primer' to the surface of the moisture-proof reinforced top coat layer, the process of attaching a patterned paper to the surface of the cured undercoat layer, and the pattern paper In the painting stage of the floor pattern applying the top coat of 'non-slip poly top' with color tone; It is composed of a combination, and the floor is moisture-proof reinforced by a primer layer and a topcoat layer, and a floor pattern of a contrasting tone is created by the topcoat layer of the 'poly top' and the two topcoat layers of the 'non-slip poly top'. As a result, the durability of the floor is improved and a more beautiful floor pattern can be painted.
priorityDate 2019-12-23-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101267433-B1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101148076-B1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101461172-B1
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419512635
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID962

Total number of triples: 23.