Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b9a913b2c592e6429474cc701cad3171 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_fd48dcb63fc0cb5fb5ec2bface8c32c1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c999e0587b16b2b6a3db01eeefd9d74d |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-91 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-70 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B18-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B22-0093 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B22-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K17-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B18-064 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B18-141 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B111-70 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B18-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B18-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B18-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B22-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B22-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K17-08 |
filingDate |
2020-11-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2021-05-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_85d1409cbcc8121d6cd212cda41270c5 |
publicationDate |
2021-05-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-102255382-B1 |
titleOfInvention |
Manufacturing method of environment-friendly grouting chemical liquid and construction method using the same |
abstract |
The present invention relates to an eco-friendly grouting chemical manufacturing method and a grouting construction method using the same, which prevents environmental pollution due to toxicity of cement by not using cement, and prevents alkali elution by excluding the use of sodium silicate (water glass). It has its purpose. To this end, the present invention comprises the steps of: (a) preparing an inorganic powder A medicine containing silica-based by-products as a main component (S10); (b) dissolving the inorganic drug A powder prepared in step S10 in water to prepare a liquid inorganic drug A (S20); (C) preparing a gypsum-based drug B powder having a gypsum-based by-product as a main component (S30); (d) dissolving the gypsum-based drug B powder prepared in step S30 in water to prepare a liquid gypsum-based drug B (S40); (e) preparing a silica aluminum sol by mixing and reacting the inorganic chemical A and the gypsum chemical B (S50); (f) reacting the aluminum silica sol prepared in step S50 with calcium ions to prepare a calcium aluminum silicate gel (S60). |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102386363-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102435537-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102435539-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102454865-B1 |
priorityDate |
2020-11-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |