Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4de0c9cba467a04987c9bbe8c7316b8c |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2995-006 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2067-046 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29L2031-712 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-022 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L67-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-80 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-013 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-5415 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-82 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-0025 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K67-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L31-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-5415 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-013 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-82 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-80 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C48-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C48-03 |
filingDate |
2020-09-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2021-04-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_23f8fde2beba490abcfdd338cf0cf78f |
publicationDate |
2021-04-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-102243815-B1 |
titleOfInvention |
A method for processing eco-friendly plastic material |
abstract |
An embodiment of the present invention includes a first step of introducing a first polylactic acid, an alkoxyvinylsilane, a crosslinking catalyst, and a polymerization catalyst into the main feeder of the first extruder; A second step of injecting an inorganic filler into the side feeder of the extruder; A third step of reacting and extruding at 150 to 200°C; A fourth step of introducing the reaction extrudate and the second polylactic acid into a second extruder; And it provides a processing method of an eco-friendly plastic material comprising a; and a fifth step of molding extrusion at 180 ~ 245 ℃. |