http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102240535-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D10B2321-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-54 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2203-12 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01F21-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L33-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01F25-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D4-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D5-06 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01D1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-18 |
filingDate | 2015-01-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2021-04-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2021-04-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-102240535-B1 |
titleOfInvention | Process for the production of acrylic fibers |
abstract | A process for preparing a homogeneous spinning solution for producing acrylic fibers is described, comprising the following steps: i) a powder homopolymer or copolymer of acrylonitrile at a temperature in the range of 5° C. to 10° C., a mixture of DMSO/water in the range of 94.5/5.5 to 97/3% w/w, preferably DMSO/ at a temperature of 5° C. Preparation of a homogeneous suspension by mixing with a mixture of 95/5 water, said mixing decomposing a stream of DMSO/water solvent for a time in the range of 5 to 30 minutes and premixed powder homopolymers or copolymers of acrylonitrile Carried out by spraying the stream of; ii) heating the homogeneous suspension from step i) to a temperature in the range of 70° C. to 150° C. for a time in the range of 0.5 to 30 minutes until complete dissolution of the homopolymer or copolymer and formation of a homogeneous solution. This spinning solution is then supplied to a storage tank or spinning line. |
priorityDate | 2014-01-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 46.