abstract |
A propylene-based resin (A), a propylene-based resin (B) containing at least a carboxylate bonded to a polymer chain, and a reinforcing fiber (C), and the propylene-based resin (A) has a weight average molecular weight of 150,000 or more. The component (A-1) contains more than 70% by mass and 100% by mass or less, and the amount of the propylene-based resin (B) is 3 to 50 parts by mass with respect to 100 parts by mass of the propylene-based resin (A), and the propylene-based resin (A ) And the total content of the propylene-based resin (B) is 0.3 to 5% by mass of the total reinforcing fiber bundle, reinforcing fiber bundles excellent in mechanical properties and handling properties; And a molding material comprising this reinforcing fiber bundle and a matrix resin. |