http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102164738-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L33-06 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F20-68 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F220-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F220-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F6-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L33-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F120-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F20-14 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F6-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-38 |
filingDate | 2015-02-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2020-10-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2020-10-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-102164738-B1 |
titleOfInvention | Production method of (meth)acrylic resin composition |
abstract | A raw material solution (A) containing methyl methacrylate, an alkyl acrylate ester and a chain transfer agent at a mass ratio of alkyl acrylate/methyl methacrylate of 0/100 to 20/80, and having a dissolved oxygen concentration of 50 ppm or less was prepared. , A radical polymerization initiator, a polymerization inhibitor, and methyl methacrylate are contained, and in the presence of oxygen, a raw material liquid (B) maintained at a liquid temperature of 10° C. or lower is prepared, and a raw material liquid (A) and a raw material liquid (B) are formed. A (meth)acrylic resin composition is obtained by a method having a step of continuously supplying to a reactor, bulk polymerization at a polymerization conversion ratio of 40 to 70 mass% in a tank reactor to obtain a reaction product. |
priorityDate | 2014-02-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 111.