http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102158511-B1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f4ef10d3f7cf8c92d6b2c6d36da31428 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-382 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-2203 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-28 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D1-00 |
filingDate | 2020-06-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2020-09-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5b32ca14e4e805864b122101e8dfddf1 |
publicationDate | 2020-09-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-102158511-B1 |
titleOfInvention | Eco-friendly ceramic-based paint composition for preventing corrosion and deterioration of surface and construction method for surface protection of structure using the same |
abstract | The present invention is an eco-friendly ceramic-based coating composition for preventing surface corrosion and deterioration of a structure, based on 100 parts by weight of a titanium dioxide-tin dioxide sol; 60 to 80 parts by weight of siloxane; 30 to 50 parts by weight of boron nitride; 30 to 50 parts by weight of colloidal silica; 1 to 10 parts by weight of goetite; 1 to 10 parts by weight of lithium hydroxide; 1 to 10 parts by weight of polyoxyethylene lauryl ether; 0.1 to 5 parts by weight of sodium silicate; 0.1 to 5 parts by weight of sodium methyl silicate; And 0.1 to 5 parts by weight of butylated hydroxyanisole; With excellent strength and durability, it is possible to physically and chemically protect the surface of various structures, and it is an environment-friendly ceramic coating composition for preventing surface corrosion and deterioration of structures that can provide excellent aesthetics and roughness with room temperature curing type, and the surface of structures using the same. It relates to the protective construction method. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102288763-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102534952-B1 |
priorityDate | 2020-06-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |