http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102071588-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F10-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F210-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F4-642 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F4-6592 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F4-65927 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F10-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F210-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-642 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-6592 |
filingDate | 2015-12-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2020-01-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2020-01-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-102071588-B1 |
titleOfInvention | Olefin based polymer |
abstract | The present invention (1) Melt Index (Melt Index, MI, 190, 2.16 kg loading conditions): 0.1 to 100 g / 10 min; (2) molecular weight distribution (MWD): 1.0 to 3.0; (3) two or more melting temperatures (Tm) obtained from a DSC curve obtained by measuring with a differential scanning calorimeter (DSC); And (4) Mw = −K × log (MI) + Tm (H) × 1000, wherein the K value satisfies 20,000 <K <60,000, wherein Tm (H) is at least two melts. The present invention relates to an olefin-based polymer showing the highest melting temperature among the temperatures. The olefin-based polymer according to the present invention exhibits high molecular weight and narrow molecular weight distribution, and particularly exhibits higher molecular weight than when having the same melt index. have. |
priorityDate | 2015-12-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |