http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102070333-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2002-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2002-74 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2002-72 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-62 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01F7-785 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09C1-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01F7-005 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01F3-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G9-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01F5-24 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01F5-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G9-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01F3-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01F7-785 |
filingDate | 2016-09-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2020-01-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2020-01-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-102070333-B1 |
titleOfInvention | Hydrotalcite Particles and Manufacturing Method Thereof |
abstract | The present invention provides the hydrotalcite particles according to claim 1 and a preparation method thereof. (1) general formula [(Mg) Y (Zn) Z ] 1-X (Al) X (OH) 2 (CO 3 2- ) (x) / 2 nH 2 O In the formula, x, y, z and m are values satisfying the following conditions. 0.2 ≦ x <0.4, y + z = 1, 0.7 ≦ y ≦ 1, 0 ≦ z ≦ 0.3, 0 ≦ n <1; (2) The average primary particle size of the hydrotalcite particles has a size of 150 to 250 nm. (3) The average secondary particle size (D 50 ) of the hydrotalcite particles has a size of 1 to 2.5 μm. (4) Hydrotalcite particles have a specific surface area of 5 to 40 m 2 / g as measured by the BET method. (5) The hydrotalcite particles have a height of the first peak (2θ = 11.4 to 11.7 °) in which the X-rays are diffracted due to the presence of the plate layers on the X-ray diffraction pattern and the presence of the plate and the interlayer materials. The ratio of the height of the second peak (2θ = 23 to 24 °) which is diffracted by the line has a ratio of more than 2.10 and not more than 2.65. |