http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102024960-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J2229-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J2229-42 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J29-76 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J29-78 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C10G47-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C10G47-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J31-0201 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-002 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J37-0201 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C10G65-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J37-0236 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J29-76 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C10G47-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J37-02 |
filingDate | 2012-11-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2019-09-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2019-09-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-102024960-B1 |
titleOfInvention | Method for preparing a catalyst usable in hydroconversion and including at least one nu-86 zeolite |
abstract | The present invention relates to a process for preparing a catalyst comprising at least the following steps: a) preparing a carrier containing from 0.2 to 30% by weight of NU-86 zeolite and from 70 to 99.8% by weight of a porous inorganic matrix, wherein the weight Percentages are expressed relative to the total weight of the carrier; b) at least one impregnating said carrier prepared according to step a) with at least one solution containing, alone or in combination, at least one precursor of at least one metal selected from the group consisting of Group VIII and Group VIB metals; c) at least one ripening step; And d) at least one drying step carried out at a temperature below 150 ° C. without subsequent calcination steps. The present invention also relates to a hydrocracking process of a hydrocarbon injection using a catalyst prepared according to the above production process of the present invention. |
priorityDate | 2011-12-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 92.