abstract |
The present modifier has a continuous phase (A) containing a second polyolefin resin, a dispersed phase (B) containing a polyamide resin and a modified elastomer, and the dispersed phase (B) includes a modified elastomer having a reactive group with a polyamide resin. It consists of melt-kneaded material, and when the sum total of a continuous phase (A) and a dispersed phase (B) is 100 mass%, a dispersed phase (B) is 80 mass% or less. This usage method mixes 0.5 mass part or more and 70 mass parts or less of modifiers when 1 mass polyolefin resin is 100 mass parts. This manufacturing method is equipped with the process of melt-kneading a 2nd polyolefin resin, the polyamide resin, and the melt-kneaded material of the said modified elastomer. |