Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ff704047306b664f7af5ec798b4dd29c |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-91 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2103-404 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B22-143 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B26-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B18-167 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B18-142 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B24-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B22-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B24-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B40-0032 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B103-40 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B24-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B24-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B22-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B22-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B18-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B18-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B40-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B26-26 |
filingDate |
2018-12-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2019-08-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_aab8d75ad1a8aef10fba3518e26c8e85 |
publicationDate |
2019-08-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-102013557-B1 |
titleOfInvention |
Recycled asphalt mixtures manufactured in room temperature and menufacturing method thereof |
abstract |
The present invention relates to a room temperature asphalt concrete mixture and a method for producing the same, and more particularly, aggregate comprising a recycled aggregate obtained from waste ascone; Asphalt, surfactant, and water are mixed to have a cation, and 3.0 wt% to 8.0 wt% emulsified asphalt; In the process of mixing the aggregate and the emulsified asphalt at room temperature, a chemical additive containing 0.015% by weight to 0.03% by weight of a chemical component including a foaming agent and a surfactant that generates bubbles on the surface of the aggregate is diluted with water. ; Including, the mixture of the aggregate and the emulsified asphalt provides a homogenous asphalt concrete mixture and a method for producing the same, which exhibits high adhesion by hydrogen bonding through ion exchange of the aggregate and the emulsified asphalt. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113956844-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113956844-A |
priorityDate |
2018-12-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |