http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102008664-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-91 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2103-54 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/E04F15-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B24-383 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B14-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B14-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B18-141 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B24-2688 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B103-54 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B18-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B14-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B14-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/E04F15-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B24-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B24-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-02 |
filingDate | 2018-01-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2019-08-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2019-08-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-102008664-B1 |
titleOfInvention | High-performance tile joint material including blast furnace slag fine powder |
abstract | The present invention relates to a high-performance elastic joint material composition using blast furnace slag fine powder, which is an industrial by-product, and more particularly, by using blast furnace slag fine powder, which has excellent chemical resistance, and also adds a tripolymer reemulsifying powder resin to provide adhesion strength and The present invention relates to a high-performance tile joint material that improves bending strength and improves water resistance without deteriorating physical properties by using calcium stearate water repellent. The present invention "white portland cement 40 ~ 60wt%; Blast furnace slag fine powder 2 ~ 10wt%; Vinyl acetate / ethylene / methyl methacrylate terpolymer 2 ~ 4wt% of re-emulificaion type powder resin; Limestone fine powder 5-20 wt%; Dolomite 30-40 wt%; Methyl cellulose 0.04-0.10 wt%; Higher fatty acid metal salts 0.2-1.0 wt%; And white pigment 0.1 ~ 0.5wt%; It provides a high-performance tile joint comprising a. |
priorityDate | 2018-01-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |