Predicate |
Object |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C3-097 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61K6-033 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B32-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C10-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B27-012 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61K6-838 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61K6-0273 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C3-085 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61K6-833 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61K6-836 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61K6-0276 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03B27-012 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61K6-838 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C3-097 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C3-085 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03B32-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61K6-027 |
filingDate |
2017-03-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2019-05-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate |
2019-05-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-101975548-B1 |
titleOfInvention |
Method for preparing glass-ceramics, capable of adjusting machinability or translucency through change in temperature of heat treatment |
abstract |
The present invention relates to a method for producing a crystallized glass of lithium disilicate having a silicate as a main component, and more particularly, to a method for producing a crystallized glass capable of controlling workability or light transmittance according to the size of a crystal by using a primary heat treatment or a secondary heat treatment will be. To this end, the method for producing a crystallized glass including the silica crystal phase of the present invention is characterized in that the glass composition is subjected to a first heat treatment at 400 to 850 ° C, and a lithium disilicate crystal phase and a silica crystal phase are generated by 5 to 2000 nm by a first heat treatment . To this end, the method for producing a crystallized glass including the silica crystal phase of the present invention is characterized in that the second heat treatment is performed at 780 to 880 ° C after the first heat treatment, and the light transmittance is controlled by the temperature of the second heat treatment. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3744696-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3974396-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2022250184-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11730576-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11104600-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3974397-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-4234505-A2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-4124606-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-4104810-A1 |
priorityDate |
2017-03-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |