http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101956777-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B27K5-003 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B27K3-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B27N1-029 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B27M3-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B27K5-0085 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B27N1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B27M3-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B27K5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B27K3-52 |
filingDate | 2017-06-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2019-03-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2019-03-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101956777-B1 |
titleOfInvention | Wood panels for furniture, and a method of manufacturing the same |
abstract | Disclosure of Invention Technical Problem [8] The present invention relates to a radon reducing material, which can prevent or reduce the generation of harmful substances generated from an adhesive to prevent contamination of the indoor environment, and can emit far infrared rays using a transition metal element, To a method of manufacturing a wood panel for furniture, which can protect the user's health by forming an environmentally friendly UV primer layer and an environmentally friendly top layer without using harmful chemicals such as styrene As such, The furniture-use wood panel of the present invention comprises a core material having a surface on which an LPM layer is formed, an environmentally friendly UV primer layer formed on the LPM layer, and a component formed on the environmentally friendly UV primer layer and containing a transition metal element And 6 to 8% by weight of clay minerals, and aluminum (Al) is formed on the above-mentioned far-infrared ray emitting layer by coating and heat- A sanding sealer layer formed by mixing a granular additive mixed with 3 to 5% by weight of hydrate, 1 to 2% by weight of carbonate mineral and 1 to 2% by weight of melted slag into a sanding sealer, Wherein the environmentally friendly top layer comprises 30 to 40% by weight of an unsaturated polyester resin, 50 to 60% by weight of a monomer, 2 to 5% by weight of a photoinitiator and 0 to 5% by weight of an additive, A slurry containing 1 to 2% by weight of a carbonate mineral and 1 to 2% by weight of a molten slag, wherein the slag is composed of 67 to 80% by weight of a cobalt mineral, 8 to 16% by weight of a silicon dioxide mineral, 6 to 8% by weight of clay minerals, 3 to 5% . |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102087557-B1 |
priorityDate | 2017-06-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 46.