Predicate |
Object |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-00836 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-3225 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-3224 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-77 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-9661 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-6562 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-82 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-663 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61K6-0017 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-63488 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-486 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61K6-842 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-636 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B41-009 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B41-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B41-85 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B41-89 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61K6-024 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-63416 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B41-80 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61K6-818 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61K6-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61K6-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B41-80 |
filingDate |
2015-09-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2019-03-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate |
2019-03-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-101954791-B1 |
titleOfInvention |
Method for post-processing colored zirconium oxide ceramic |
abstract |
A step of putting the colored zirconium oxide ceramic into a heating device together with an oxygen scavenger and performing a sintering process at a preset temperature, wherein the colored zirconium oxide ceramic is obtained by coloring a zirconium oxide ceramic with a colorant containing Pr 3 + And the amount of the oxygen scavenger is an over-stoichiometric value with respect to the amount of oxygen in the heating apparatus. These technical solutions may completely replace the Fe 3 + Pr 3 + in order to color the zirconium oxide ceramic in yellow. |