http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101948422-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-21 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-304 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B37-153 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B37-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-914 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-365 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-308 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B37-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B37-15 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-08 |
filingDate | 2017-05-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2019-02-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2019-02-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101948422-B1 |
titleOfInvention | Method for manufacturing resin laminate |
abstract | [PROBLEMS] To provide a method for producing a resin laminate excellent in transparency. A method for producing a resin laminate having at least an intermediate layer (A) and thermoplastic resin layers (B) and (C) present on both sides of the intermediate layer (A) Wherein the intermediate layer (A) is formed of the resin composition (a), the thermoplastic resin layers (B) and (C) are formed of thermoplastic resins (b) and (c) The method includes a step of discharging a molten resin laminate formed from at least a molten resin composition (a), thermoplastic resins (b), and (c) The resin composition (a) comprises 10 to 90 mass% of a (meth) acrylic resin and 90 to 10 mass% of a vinylidene fluoride resin based on the total resin contained in the resin composition (a) ) The weight average molecular weight (Mw) of the acrylic resin is 100,000 to 300,000, Wherein the average cooling rate from the discharge temperature to 100 占 폚 is 2.5 占 폚 / sec or more in the above step. |
priorityDate | 2016-05-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |