Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_86eaaff01673317d0984c08eb9f41709 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D101-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D7-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K9-0081 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-67 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D3-0254 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D5-12 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D5-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D101-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05K9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D3-02 |
filingDate |
2018-01-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2019-01-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_603f29380bea5cdbccd45c62a7f39573 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_da39c407781d2b4dd42955c6e5d23676 |
publicationDate |
2019-01-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-101935052-B1 |
titleOfInvention |
Manufacturing method for electro-magnetic interfernce shielding film and electro-magnetic interference shielding film using the same |
abstract |
The present invention provides a method for preparing a polymer solution, comprising the steps of: a) dissolving a cellulose-based polymer in water to prepare a polymer solution; b) adding carbon nanotubes, copper-nickel core-shell nanoparticles having an average particle diameter of 60 to 70 nm, copper-silver core-shell nanoparticles having an average particle diameter of 30 to 40 nm and a surfactant to the polymer solution, To produce a first composition for an electromagnetic wave shielding film; c) mixing the composition with carbon black, and stirring the mixture with a paste mixer to prepare a second composition; And d) applying and drying the second composition on a substrate, wherein in step b), the copper-nickel core-shell nanoparticles and the copper-silver core-shell nanoparticles have a weight ratio of 1: 2 to 2.5 To the electromagnetic wave shielding film. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20230039353-A |
priorityDate |
2018-01-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |