abstract |
A) an ethylene polymer composition having a melting enthalpy? H fus of 60 J / g or more as measured by differential scanning calorimetry at a heating rate of 20 ° C per minute, A) an ethylene polymer composition having a solubility in xylene at 25 ° C of XS A , , 25 to 55% of an ethylene polymer in an amount of 10% or less; B) a copolymer of ethylene and propylene containing ethylene in an amount of 60% or more, relative to the weight of B), of 45% to 70% and a soluble fraction XS B in xylene at 25 ° C, 45 to 75% of the coalescent, wherein all percentages are by weight; Wherein the amounts of A) and B) are based on the total weight of A) + B). |