http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101767801-B1

Outgoing Links

Predicate Object
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2307-40
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2307-304
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2307-416
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2307-42
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-36
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B9-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-0875
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B1-04
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B9-045
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B1-14
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B33-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-208
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C14-08
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C14-086
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-26
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-282
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C14-14
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/E06B3-6715
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B9-041
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-26
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-20
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/E06B3-67
filingDate 2014-01-30-04:00^^<http://www.w3.org/2001/XMLSchema#date>
grantDate 2017-08-11-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationDate 2017-08-11-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber KR-101767801-B1
titleOfInvention Infrared reflective film
abstract The infrared ray reflection film (100) of the present invention comprises an infrared ray reflection layer (20) and a transparent protection layer (30) in this order on a transparent film base (10). The infrared ray reflective layer 20 is formed from the side of the transparent film base 10 to the first metal oxide layer 21; A metal layer 25 mainly composed of silver; And a second metal oxide layer 22 composed of a composite metal oxide containing zinc oxide and tin oxide in this order. The transparent protective layer 30 is in direct contact with the second metal oxide layer 22. The thickness of the transparent protective layer 30 is preferably 30 nm to 150 nm, and is preferably an organic material layer having a crosslinked structure derived from an ester compound having an acidic group and a polymerizable functional group in the same molecule. The content of the structure derived from the ester compound in the transparent protective layer 30 is preferably 1 wt% to 40 wt%.
priorityDate 2013-01-31-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID449871035
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID411550722
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419523934
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID1004
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID411285781
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419559192
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID159575533
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID166598
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID29011
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID14806
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID450862749
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID66390

Total number of triples: 44.