http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101752034-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-3025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F2201-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-133528 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F2202-28 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G59-226 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J163-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G59-223 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L63-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-1335 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J163-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J171-00 |
filingDate | 2012-03-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-06-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-06-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101752034-B1 |
titleOfInvention | Laminate optical member and polarizing plate using photocurable adhesive |
abstract | A polarizing plate comprising a polyvinyl alcohol polarizer and a transparent protective film bonded to the polarizer through an adhesive, wherein the adhesive contains 100 parts by weight of the photo cationic curing component (A), 100 parts by weight of the photo cationic polymerization initiator (B) 1 to 10 parts by weight of the photocathode curing component (A), and the photocathode curing component (A) is formed of a photocurable adhesive containing the following amounts of (A1) to (A3) based on the total amount thereof. 30 to 85% by weight of an alicyclic diepoxy compound (A1) represented by the following formula (I); 1 to 69% by weight of a diglycidyl compound (A2) represented by the following formula (II) and Z has a branched structure; And 1 to 69% by weight of the monofunctional epoxy compound (A3) represented by the following formula (III). When the protective film is immersed in the photocurable adhesive for 2 days at 23 占 폚, the weight loss of the protective film is 0 to 30% by weight. |
priorityDate | 2011-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |