http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101700241-B1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_39119da8c171afda93e952b53629ba24 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-1216 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D1-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B08B3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D7-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D3-007 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D3-002 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D133-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-1233 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/E04F15-12 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B08B3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D1-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D133-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/E04F15-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-12 |
filingDate | 2016-09-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-01-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_44403bc6f8efe8cb2b9ca6373e03183b |
publicationDate | 2017-01-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101700241-B1 |
titleOfInvention | Floor coating method using floor coating agent having excellent brightness and hardness |
abstract | The present invention relates to a floor coating method using an eco-friendly floor coating agent for floor construction with improved lightness and hardness. Accordingly, the technical point of the present invention is to allow a coating layer having excellent lightness and hardness to be applied to a floor tile of a large-sized mart or various buildings (such as schools, airports, dormitories, public institutions or business sites) The present invention is characterized in that productivity and economical efficiency are greatly improved due to excellent restoration ability compared to a simple work process as well as cost reduction by preventing surface damage and remarkably improving previous frequent restoration work. Accordingly, the floor coating agent of the present invention is excellent in the lightness and hardness without using the marble coating agent of the present invention registered in the Japanese Patent No. 10-1583521 previously registered by the applicant of the present application. It is environment-friendly and has the properties required for flooring such as hardness, abrasion resistance, scratch resistance, And the like, and is also excellent in terms of economy. Among the PVC tiles, deluxe tiles (type in which wax is absorbed when asbestos is coated on the surface and wax is absorbed) or decor tiles (type in which wax coating is not necessary since the surface is coated with UV coating or glass) It is a feature that can be coated without. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110145094-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10759961-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101858603-B1 |
priorityDate | 2016-09-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 53.