http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101684810-B1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1bc8d5b80410c3a0594da023cfabcbe0 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2301-10 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C55-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C55-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-1545 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C55-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C55-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-1545 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 |
filingDate | 2015-12-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-12-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c094eca2863f02e45ea422c01a36211f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d2f4db4b2049d8da42446d2cfd66117a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_93d394fd9570e010b6aeac3c04fe1508 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8ed7b7475d686b8133fe83f0daf27481 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_473e619e7a0fb9a115ce8c5b34d658f2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4d1aeae0418e407a52c9d94710c41d51 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f45b31c36fc23f8eb002f03ee474ba37 |
publicationDate | 2016-12-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101684810-B1 |
titleOfInvention | Cellulose ester film having an improved barrier property at high temperature/humidity condition and method for preparing the same |
abstract | The present invention relates to an asymmetric ester compound containing an aromatic group represented by the following formula (1) capable of improving the reliability of high temperature and high humidity of a retardation film for VA (Vertical Alignment) having high reliability and a cellulose ester phase difference film capable of producing a polarizing plate A cellulose ester film comprising a plasticizer containing a saccharide compound represented by the general formula (2), and a process for producing the same. [Chemical Formula 1] T + [D + P] n + D Wherein T represents a benzene carboxylic acid residue, D represents an alkylene glycol residue having 2 to 12 carbon atoms, an aryl glycol residue having 6 to 12 carbon atoms, or an oxyalkylene glycol residue having 4 to 12 carbon atoms, An alkylene dicarboxylic acid residue of 12 to 12 carbon atoms or an aryl dicarboxylic acid residue of 6 to 12 carbon atoms, and n represents an integer of 1 or more. The benzene carboxylic acid residue is preferably a toluene acid residue, and the alkylene glycol residue is preferably selected from the group consisting of propylene glycol, neopentyl glycol, diethyleneglycol, dipropyleneglycol, Triethyleneglycol residue, and the aryl dicarboxylic acid residue is preferably a phthalic acid residue. (2) Here, R is substituted with 7 to 8 benzoic acids among the total of 8 substituents as substituents, and the unsubstituted R remains as the H group. |
priorityDate | 2015-12-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |