Predicate |
Object |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2207-04 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-3445 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-3472 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F210-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-16 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-3472 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-3445 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F210-16 |
filingDate |
2015-03-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2016-12-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate |
2016-12-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-101682047-B1 |
titleOfInvention |
Polyolefin thermoplastic elastomer having self healing properties and method of making the same |
abstract |
The present invention relates to a polyolefin thermoplastic elastomer having self-healing properties and a process for producing the same, which comprises 100 parts by weight of a polyolefin rubber grafted with 0.5 to 2.0% by weight of maleic anhydride and having a degree of crystallinity of 5 to 10% And 3 to 10 parts by weight of a hydrogen bond former comprising an amine group which reacts with an acid to form a hydrogen bond. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-4197778-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102304589-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-102021214710-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20190023206-A |
priorityDate |
2015-03-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |