http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101681961-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P20-582 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/E01C7-182 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/E01C7-265 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L95-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/E01C7-18 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/E01C7-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/E01C7-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L95-00 |
filingDate | 2015-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-12-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2016-12-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101681961-B1 |
titleOfInvention | Development of Material and Application for urgent pavement maintenance using Reclaimed Asphalt Aggregate and Quick setting reactive emulsified asphalt binder |
abstract | The present invention relates to a recycled aggregate mixture using a spherical reactive refinement emulsion binder and a pavement emergency maintenance method using the same. The object of the present invention is to provide a recycled aggregate mixture using a recycled aggregate and a spherical reactive refinement emulsion binder, wherein the aging of the pavement is severe, The present invention provides a pavement maintenance method using a recycled aggregate and a low speed reactive modified emulsion binder capable of quickly ensuring the durability of a pavement. The present invention relates to a recycled aggregate mixture containing a reduced-diameter reactive modified emulsion binder and a pavement emergency maintenance method using the same. The above-mentioned reduced-diameter reactive recycled aggregate mixture comprises 3 to 13 parts by weight of a low-molecular-weight reactive modified emulsion binder, 1 to 5 parts by weight of a reaction product, and 1 to 7 parts by weight of water, based on 100 parts by weight of the recycled aggregate, A cutting step of cutting the part; A base treatment step of cleaning and tack coating the cut surface; The pavement road is urgently maintained by the step of forming a recycled aggregate mixture layer for laying the recycled aggregate mixture on the surface treated. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2023191208-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102438241-B1 |
priorityDate | 2015-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 31.