http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101677319-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F279-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L55-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F279-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-12 |
filingDate | 2014-02-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-11-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2016-11-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101677319-B1 |
titleOfInvention | Manufacturing method of thermoplastic resin having good heat resistance |
abstract | The present invention relates to a method for producing a thermostable ABS copolymer, which comprises adding an ABS copolymer latex to coagulate the thermostable SAN copolymer latex which can be used in the production of a heat resistant ABS copolymer, thereby making it possible to coagulate relatively low temperature, Which is obtained by polymerizing a vinyl aromatic monomer and a vinyl cyan monomer having an alpha-alkylstyrene content of not less than 50% by weight to obtain a styrene-acrylate-based copolymer A method for producing a copolymer, comprising: (1) a polymerization step of copolymerizing the vinyl aromatic monomer and the vinyl cyan monomer; And (2) 1 to 49% by weight of an ABS resin latex to 51 to 99% by weight of the SAN resin latex obtained in the above polymerization step, and mixing the 100% by weight of the mixed SAN resin latex with the ABS resin latex, And 1 to 5 parts by weight of a surfactant. |
priorityDate | 2013-09-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |