http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101667967-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M2220-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P70-50 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-58 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-623 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-625 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-131 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-1391 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-505 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-131 |
filingDate | 2013-08-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-10-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2016-10-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101667967-B1 |
titleOfInvention | Cathode slurry for electrochemical device, cathode manufactured using the slurry, and a method of making the cathode |
abstract | The present invention relates to a method for manufacturing a positive electrode slurry for an electrochemical device, which comprises mixing a metal salt together with a positive electrode active material, a binder and a conductive material to reduce time and cost in the manufacturing process, A cathode for an electrochemical device, an electrochemical device including such a cathode, and a method for manufacturing the anode. In the anode of the present invention, metal oxide is uniformly coated on the surface of the cathode active material, The side reaction between the positive electrode active material and the electrolyte generated during the charging and discharging of the battery is effectively blocked to reduce the dissolution or degradation of the positive electrode, ultimately improving the battery life characteristics. |