http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101629945-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B22-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B40-0039 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B40-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B40-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B22-124 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B22-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B40-025 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B40-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B40-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B22-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B22-10 |
filingDate | 2011-04-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-06-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2016-06-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101629945-B1 |
titleOfInvention | Composition of saving cement and curing method of high strength thereby |
abstract | The present invention can significantly reduce the amount of cement used and maintain the strength over the existing strength, and it is possible to reduce the cement cost by 30 ~ 50% To a high strength curing method. The cement reducing agent according to the present invention comprises 10-15 parts by weight of potassium chloride, 10-15 parts by weight of sodium chloride, 5-10 parts by weight of ammonium chloride, 1-5 parts by weight of nickel chloride, 1-5 parts by weight of cobalt chloride, 20 to 30 parts by weight of potassium carbonate, and 5 to 15 parts by weight of boric acid. |