http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101602531-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F279-02 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L55-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F279-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F279-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29B11-10 |
filingDate | 2013-07-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-03-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2016-03-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101602531-B1 |
titleOfInvention | Manufacturing method of transparent thermoplastic resin having no mold deposit |
abstract | The present invention relates to a method for producing a transparent thermoplastic resin which is excellent in transparency, impact strength and processability and does not cause mold deposit during high-speed continuous injection molding. The present invention relates to: (1) a method for producing a transparent thermoplastic resin from a conjugated diene monomer A step of preparing a rubber latex to produce a rubber latex; (2) a step of producing a resin latex to produce a resin latex by graft copolymerizing a (meth) acrylic acid monomer, an aromatic vinyl monomer and a vinyl cyan monomer to the rubber latex using an initiator; (3) agglomerating the resin latex to obtain a wet powder; And (4) wet co-extruding the wet powder together with the aromatic vinyl-based copolymer to produce pellets. |
priorityDate | 2013-07-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |