http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101592051-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-052 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-136 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B25-45 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-5825 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-136 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-052 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B25-45 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-58 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B1-06 |
filingDate | 2009-04-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-02-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2016-02-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101592051-B1 |
titleOfInvention | Process for the preparation of crystalline lithium-, iron- and phosphate-comprising materials |
abstract | The present invention relates to a process for the preparation of a compound of general formula (I) Li ab M 1 b Fe 1-c M 2 c P de M 3 e O x (I) Wherein M 1 , M 2 , M 3 , a, b, c, d and e have the following meanings: M 1 : Na, K, Rb and / or Cs, M 2 : Mn, Mg, Ca, Ti, Co, Ni, Cr and / or V, M 3 : Si and / or S, a: 0.8 - 1.9, b: 0 - 0.3, c: 0 - 0.9, d: 0.8-1.9, e: 0 - 0.5, x: 1.0 - 8 (depending on the amount and oxidation state of Li, M 1 , Fe, M 2 , P, and M 3 ) ) The compound of general formula (I) is neutral charged; The method comprises the following steps: (A) one or more lithium-containing compounds, one or more iron-containing compounds wherein iron has an oxidation state of +3, and, if present, one or more M 1 -containing compounds and / A mixture comprising at least one of the above M 2 -containing compounds and / or at least one M 3 -containing compound, if present, and at least one compound comprising at least one phosphorus atom present in oxidation state +5 , ≪ / RTI > (B) optionally, drying the mixture provided in step (A) to obtain a solid compound, and (C) calcining the solid compound obtained from the step (A) or the step (B) at a temperature of 300 to 1000 캜 Lt; / RTI > |