http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101590854-B1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_57e98c023a56313fd00216b9bf666886 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2207-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-91 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02A30-30 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L95-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B24-2676 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B18-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B24-16 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B24-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B18-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L95-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B24-16 |
filingDate | 2015-10-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-02-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_99fc16a1b03f53f6ca324f7123955076 |
publicationDate | 2016-02-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101590854-B1 |
titleOfInvention | Modified recycle warm-mix asphalt mixture and manifacturing method of the same |
abstract | The present invention relates to a modified regenerated mesophase asphalt mixture which recycles waste asbestos and significantly reduces the production temperature of the heated asphalt during the production process, thereby reducing emissions of environmental pollutants and significantly improving the mechanical properties, aging resistance and storage stability of the packaged road And a manufacturing method thereof. The modified regenerated mesophase asphalt mixture of the present invention comprises: a fresh aggregate; A recycled aggregate and waste asphalt, and having a weight ratio of 0.1 to 50 parts by weight based on 100 parts by weight of the new aggregate; And a regenerated asphalt composition containing 0.1 to 10 parts by weight, based on 100 parts by weight of the new aggregate, of a polymer containing neopentylsulfone, free sulfur, inorganic acid and styrenic block copolymer and restoring the physical properties of the waste asphalt, The regenerated asphalt composition includes a release reducing agent for promoting the bond between the aggregate containing the new aggregate and the recycled aggregate and the asphalt including the fresh asphalt and the waste asphalt, A viscosity adjusting agent for lowering the viscosity of the asphalt and the waste asphalt, and a rapid curing agent for shortening the curing time of the modified regeneration heavy-duty asphalt mixture. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108084718-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101906757-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101977583-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102115296-B1 |
priorityDate | 2015-10-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 62.