http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101575221-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D201-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D201-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-12 |
filingDate | 2013-12-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-12-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2015-12-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101575221-B1 |
titleOfInvention | Process for producing a co-solvent containing graphite oxide coating liquid and a process for producing a graphite oxide coating |
abstract | The present invention relates to a process for producing a graphite oxide coating liquid in which the plate-like structure of graphite oxide is maintained by replacing water molecules on the surface of graphite oxide with a desired solvent without heat treatment, and a process for producing graphite oxide coatings based thereon. (A) oxidizing graphite to produce a water-based graphite oxide slurry; (b) preparing a solution in which an excess amount of an amphoteric solvent is added to the aqueous graphite oxide slurry; (c) providing molecular shock waves to said solution; (d) repeating the steps (b) and (c) two or more times to prepare a coating solution; And (e) adding an amount of cosolvent to the coating solution; Containing graphite oxide coating liquid, which is characterized in that it contains a " co-solvent containing graphite oxide coating liquid ". |