http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101573927-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F22-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03F7-028 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03F7-027 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-028 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-027 |
filingDate | 2008-11-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-12-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2015-12-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101573927-B1 |
titleOfInvention | Colored photosensitive resin composition |
abstract | The present invention relates to a photosensitive resin composition comprising a colorant (A), an alkali-soluble resin binder (B), an acrylic-based photopolymerizable monomer (C) having an ethylenically unsaturated double bond, a photopolymerization initiator (D), an additive (F) The alkali-soluble resin binder (B) comprises i) at least one binder having a weight average molecular weight of 20,000 to 30,000 and an acid value of 85 to 120; And ii) at least one kind of binder having a weight-average molecular weight difference of 100 to 10,000, and i) a difference between a binder and an acid value of 1 to 30, and ii) at least one kind of binder .n n n The colored photosensitive resin composition according to the present invention forms a pattern different from the conventional one by using two or more kinds of alkali-soluble resin binders having different degrees of curing at the time of exposure. Accordingly, it is possible to form a colored coating layer of an excellent complementary metal oxide semiconductor image sensor by preventing the occurrence of missing, missing, and remaining on the substrate during the implementation of the fine pattern and during development.n n n n A colored photosensitive resin composition, a color filter, a CMOS (Complementary Metal Oxide Semiconductor), a CIS, a liquid crystal display element, |
priorityDate | 2008-11-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 464.