abstract |
A first resin; And a second resin, wherein the second resin is an alkyl group having 2 to 20 carbon atoms; An alicyclic ring having 5 to 40 carbon atoms; And an aromatic ring having 6 to 40 carbon atoms, wherein a difference in melt viscosity between the first resin and the first resin is 100 to 1000 s -1 And a glass transition temperature (Tg) difference of 10 ° C to 150 ° C, a method for producing a resin molded article using the same, and a resin molded article obtained therefrom The resin mixture can improve the mechanical properties and surface characteristics of a molded article and omit the additional surface coating step, thereby shortening the process time, increasing the productivity, and reducing the production cost. |