http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101554864-B1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_27087d6b6d5b7154e00caa267e266fd6 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B24-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B24-38 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B24-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B24-24 |
filingDate | 2014-11-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-09-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_20e4182bb80ad3ae095ad118fc32c981 |
publicationDate | 2015-09-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101554864-B1 |
titleOfInvention | A preparation method of concrete with a precipitation agent for recovered remocon water and concrete made thereby |
abstract | The present invention relates to a sedimentation accelerator for recovered concrete containing recovered water containing 10 to 20 parts by weight of a dilution of a cellulose-based thickener based on the total weight and 45 to 46 parts by weight of a silicone-based defoaming agent, And the generation of bubbles is reduced. When the sludge settlement promoter prepared by the method of manufacturing the sludge settlement promoter of the ready-mixed recovered water proposed in the present invention is used, it is possible to effectively prevent the phenomenon that the foam is mixed with the sludge generated in the ready- By rapidly aggregating the solids in the sludge and depositing it below the recovery water storage tank, it is possible to increase the substantial storage capacity of the ready-mixed recovery water storage tank and minimize the inflow of sludge solid content when using the ready-mixed recovery water, There is an advantage that it is possible to manufacture the concrete more economically and to provide an environmentally-friendly concrete production method. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112645629-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20220105706-A |
priorityDate | 2014-11-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 518.