http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101538967-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25B15-021 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25B1-01 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25B15-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25B11-061 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25B9-65 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25B1-00 |
filingDate | 2014-01-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-07-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2015-07-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101538967-B1 |
titleOfInvention | Manufacturing method of metal oxide powder |
abstract | The present invention relates to a method for producing a polymer electrolyte membrane, comprising the steps of: adding deionized water and an electrolyte to a reactor and stirring to form an electrolyte aqueous solution; immersing a first base material made of a metal or metal alloy material to be reacted in the electrolyte aqueous solution, Connecting a second base material made of a metal or a metal alloy material having a smaller oxidation-reduction potential to the first base material and higher in corrosion resistance than the first base material to the negative electrode of the power supply; The method comprising: setting a voltage difference between substrates and operating the power supply to cause an oxidation reaction to start in the first substrate; forming an arc plasma on the surface of the first substrate, A metal oxide is formed on the surface of the first base material and is separated from the surface of the first base material, A step of selectively precipitating a precipitate that is sitting in the aqueous electrolyte solution, and a step of heat treating the precipitate selectively separated in an oxidizing atmosphere to obtain a metal oxide powder . According to the present invention, since no strong acid is used and a small amount of electrolyte and deionized water are used, there is little harmful substances or wastewater that can be generated during the process, and it is eco-friendly and cost-saving and mass production in a short time is possible . |
priorityDate | 2014-01-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |