http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101523627-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-035 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02T10-86 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08C19-44 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L93-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B60C1-0016 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L15-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L83-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L9-06 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L93-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08C19-25 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B60C1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L15-00 |
filingDate | 2013-02-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-05-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2015-05-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101523627-B1 |
titleOfInvention | Rubber composition for tire treads |
abstract | A rubber composition for a tire tread is provided which is improved in low rolling resistance, wet performance and abrasion resistance to a level higher than a conventional level. Modified conjugated diene terpene resin is contained in an amount of 3 to 60 parts by weight and a filler in an amount of 100 to 150 parts by weight in 100 parts by weight of a diene rubber containing 35 to 89% by weight of a diene polymer rubber and 11 to 40% by weight of a butadiene rubber And the ratio Wte / Wbr of the amount of the butadiene rubber blended Wbr to the blended amount of the aromatic modified terpene resin is 0.5 to 1.3, and the interaction of the modified conjugated diene polymer rubber with silica Wherein the modified conjugated diene polymer rubber has an aromatic vinyl unit content of 38 to 48% by weight, a vinyl unit content of 20 to 35% by weight, a weight average molecular weight of 600,000 to 1,000,000, The aromatic modified terpene resin has a softening point of 100 to 150 ° C. |