http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101508192-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09C1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09C3-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61K8-19 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09C3-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09C1-00 |
filingDate | 2013-07-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-04-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2015-04-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101508192-B1 |
titleOfInvention | Manufacturing Method for used Hydro-Thermal Synthesis of the Magnesium Hydroxide on the Flat Pigment Coated with Magnesium oxide and Development for Soft Focus Cosmetics Substrate Used Method |
abstract | The present invention relates to a method for treating a surface of a material such as mica, sericite and alumina, which are plate-like pigments, using magnesium hydroxide (Mg (OH) 2 ) produced by hydrothermal synthesis using microwave, To a cosmetic composition. The pigment having soft-focus effect by surface treatment of mica and sericite alumina which are plate-like pigments using the magnesium oxide of the present invention can express a natural appearance which does not accompany color expression power, persistence and gloss similar to those of existing pigments And is superior in skin safety and formulation stability, so that it can be more useful than pigments having a conventional soft focus effect. |