http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101493444-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D10B2509-00 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y30-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y40-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y10-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61K9-1647 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D5-003 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D5-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D04H1-728 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L27-14 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01D5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-62 |
filingDate | 2014-02-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-02-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2015-02-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101493444-B1 |
titleOfInvention | Polycaprolactone nano-fibers comprising physiological active substance and manufacturing method thereof |
abstract | Disclosed is a polycaprolactone nanofiber containing a physiologically active substance and a method for producing the same. The method for producing a polycaprolactone nanofiber containing a physiologically active substance according to the present invention comprises: 5 to 30 parts by weight of polycaprolactone and 0.5 to 10 parts by weight of Poloxamer, based on 100 parts by weight of the first solvent, To prepare a first solution; 0.5 to 5 parts by weight of sodium alginate based on 100 parts by weight of the second solvent and dissolving the physiologically active substance to prepare a second solution; Mixing and stirring the first solution and the second solution to prepare an emulsion solution in which the second solution is dispersed in the first solution; And electrospinning the emulsion solution to produce nanofibers. According to the present invention, the physiologically active substance can be contained in the nanofiber by a simple process through a single electrospinning, the denaturation of the physiologically active substance can be minimized, The release rate of the active material can be controlled in various ways. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11738116-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113373595-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104807859-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3917478-A4 |
priorityDate | 2014-02-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 37.