classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22F2301-255 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22F2304-05 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22F9-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22F1-0547 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22F9-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82B3-00 |
filingDate | 2013-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-01-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2015-01-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101478076-B1 |
titleOfInvention | Metal NANOWIRE AND METHOD FOR MANUFACTURING THE SAME |
abstract | The present invention relates to a metal nanowire having an improved aspect ratio and a method of manufacturing the same, and more particularly, to a metal nanowire having a small diameter and a long length, and a method for manufacturing a metal nanowire having an improved yield. A method of manufacturing a metal nanowire includes: mixing at least two solvents having different reducing powers; Adding a capping agent having different molecular weights to the solvent; Adding a catalyst to the solvent to which the capping agent is added; Preparing a reaction solution in which metal nanowires are formed by adding a metal oxide to a solvent to which a catalyst is added; Adding a solvent at room temperature to the reaction solution; And purifying the reaction solution to obtain metal nanowires. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101884299-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20180004862-A |
priorityDate | 2013-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |