http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101476223-B1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8b2e06470f83ff23ef7282eadea6a68f |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-62 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G65-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J11-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J11-18 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G65-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J11-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J11-18 |
filingDate | 2013-12-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2014-12-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_57a93a1da8e862ca43eea3d78517ca89 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d5b5229c1804b5d678d11f32ebb2b22c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bc74d5c3bf684e0db3fa47f2c1600d57 |
publicationDate | 2014-12-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101476223-B1 |
titleOfInvention | Recovering method highly efficiently from waste polyurethane using recycled polyol |
abstract | The present invention relates to a method for recovering a waste polyurethane as a polyol by a glycol depolymerization reaction, and more particularly, to a method for recovering a waste polyurethane from a waste polyurethane using a recycled polyol. More specifically, 50 to 200 parts by weight of regenerated polyol and 50 to 500 parts by weight of glycols, and heating and stirring at 120 to 300 ° C .; Adding 50 to 150 parts by weight of an amine-based oligomer and the vegetable oil, 0.1 to 50 parts by weight of an organometallic catalyst or an amine catalyst to the mixture of the first stage and reacting at a temperature of 170 to 400 ° C; And a third step of sufficiently reacting the mixture of the second step to convert the waste polyurethane into a polyol due to glycol depolymerization and then adding 0.001 to 10 parts by weight of an anti-emulsifier at a temperature of 160 to 180 ° C. The present invention relates to a high-efficiency recovery method of polyol from waste polyurethane. |